Standard: GB/T714-2014
Grades: Q500qD, Q500qE, Q500qF
Category: Bridge structural steel plate
Chemical composition of Q500qD, Q500qE, Q500qF steel plates
Grades |
C |
Si |
Mn |
P |
S |
Nb |
V |
Ti |
Cr |
Ni |
Cu |
Mo |
N |
Als |
Q500qD |
≤0.11 |
≤0.55 |
0.80-1.70 |
≤0.025 |
≤0.015 |
0.005-0.060 |
0.010-0.080 |
0.006-0.030 |
≤0.80 |
≤0.70 |
≤0.30 |
≤0.30 |
≤0.0080 |
0.010-0.045 |
Q500qE |
≤0.11 |
≤0.55 |
0.80-1.70 |
≤0.020 |
≤0.015 |
|||||||||
Q500qF |
≤0.11 |
≤0.55 |
0.80-1.70 |
≤0.015 |
≤0.015 |
Q500qD, Q500qE, Q500qF mechanical properties
Grades |
Tensile requirement |
V-shaped impact test |
||||
yield strength/MPa, min |
Tensile strength/MPa |
Elongation, A% |
Test temperature/℃ |
Impact absorption energy/J |
||
Thickness/mm |
||||||
≤50 |
50-100 |
|||||
Min. |
Min. |
|||||
Q500qD, Q500qE, Q500qF |
500 |
480 |
630 |
18 |
-20 |
120 |
-40 |
||||||
-60 |
47 |
IF you are looking for Q500qD, Q500qE, Q500qFstructural steel for bridges, welcome to contact us.