Different from ordinary steel plates, corten A weathering steel plates have good corrosion resistance. Under severe weather such as acid rain, many buildings began to show different degrees of corrosion, which not only affected the buildings, but also affected the people in the buildings. At the same time it also brings some security risks. The weather resistance of corten A weathering steel plate during construction also slowed down the corrosion of the building, and achieved good application effects. Let's take a look at the steps of corten A weathering steel welding.

1. Process the grooves in the welds of corten A weathering steel and stainless steel respectively.

2. After polishing and removing the dirt around the groove, match the groove of the weather-resistant plate with the groove of the stainless steel plate to form a welding area.

1 (100)

3. Non-pulsating solder is used to weld the weld zone formed between the high weather resistance plate and the stainless steel plate, and a primer layer is formed under the weld zone.

4. Non-pulsating solder is used to cover the upper surface of the soldering layer in the soldering area to form a covering layer in the soldering area. By welding corten A weathering steel plate and stainless steel plate under low current and voltage, the heat of corten A weathering steel plate and stainless steel is reduced during the welding process, the melting rate is effectively reduced by the two plates, and corten A weathering steel plate and stainless steel are manufactured. It can be fused more completely to improve the weldability of welding.

BBN Group to solve your What is the welding procedure of corten A weathering steel plate? You can also understand the common problems of all BBN Group products or services , and you can also learn about BBN Group products and services , cases .
I Want To...
Contacts
Hotline:0086-371-86151827
Latest News
More News
2025.04.17
We specialize in producing A/B/C/D grade alloy boiler plates that comply with ASTM A302 standards, including low-alloy manganese molybdenum steel se
2025.04.17
A302GrB A302Gr.B ASTM A302 grade B A302 Gr B alloy steel plate belongs to low-alloy manganese molybdenum steel, which meets the ASTM A302 standard and
Get An Instant Quotation
Please fill out the form below (required *), send us a short message, and we will contact you as soon as possible.
Product&Service
  • Metallic materials
  • Metal processing
  • Pipe processing
  • Precision casting
  • Oil and gas storage equipment
  • Environmental Engineering Services
  • Furniture Life
  • Fertilizer Production Equipments
  • Fertilizer Production Lines
Consulting online customer service
0086-371-86151827
bb@bebonchina.com
International Leading Steel Supplier
BBN continues to enhance value creation and firmly promote social harmony
Copyright © 2020 by BBN Group All rights reserved 豫ICP备19040928号-1
Online
Email
Inquiry