Measures to resolve internal cracks in weathering steel:

(1) Strictly control the overheating of the tundish according to the requirements of weathering steel, reduce the formation of small shrinkage holes inside the weathering steel bridge casting billet or reduce the development of columnar crystals.

(2) Strictly follow the standard to reduce the speed of the tundish and carry out the tail cutting operation according to the standard to ensure the internal quality of the weathering steel tailstock.

(3) To replace the mold, the foot roller and the arc section should be inspected for the arc, and the weathering steel mold and the foot roller must be inspected from time to time.

1 (61)

(4) The weathering steel should be carefully inspected for the conditions of the secondary cold water and roller table after each pouring time. If the requirements are not met, no production is allowed.

(5) The main controller of weathering steel continuous casting must keep abreast of the current fluctuation of electromagnetic stirring. If the current fluctuation of electromagnetic stirring is greater than ±10A, record the current number, start and end time, and the electromagnetic stirring cannot be turned on or the current is lower than 400A. Cut waste to standard length.

(6) If the polarization of the crystallizer is found before the machine, notify the maintenance personnel to measure the polarization amplitude of the crystallizer and adjust it in time.

(7) Constant drawing speed pouring.

BBN Group to solve your How to solve the problem of internal cracks in weathering steel? You can also understand the common problems of all BBN Group products or services , and you can also learn about BBN Group products and services , cases .
I Want To...
Contacts
Hotline:0086-371-86151827
Latest News
More News
2024.12.17
API X42 and X52 are two common pipeline steel pipe materials, mainly used for transporting liquids or gases such as oil and natural gas. The differe
2024.12.17
API 5L X52 is a carbon steel pipeline steel, which is divided into two different product specification grades, PSL1 and PSL2, according to API stand
Get An Instant Quotation
Please fill out the form below (required *), send us a short message, and we will contact you as soon as possible.
Product&Service
  • Metallic materials
  • Metal processing
  • Pipe processing
  • Precision casting
  • Oil and gas storage equipment
  • Environmental Engineering Services
  • Furniture Life
  • Fertilizer Production Equipments
  • Fertilizer Production Lines
Consulting online customer service
0086-371-86151827
bb@bebonchina.com
International Leading Steel Supplier
BBN continues to enhance value creation and firmly promote social harmony
Copyright © 2020 by BBN Group All rights reserved 豫ICP备19040928号-1
Online
Email
Inquiry